Materials used in synchronous pavement surface

Materials used in synchronous pavement surface

Summary

Materials used in synchronous pavement surface

Synchronous chip seal layer of raw materials used include two types of binders and gravel , the choice of a variety of factors need to be considered road grade , road type , traffic , weather and material supply capability. Selection of raw materials is a critical and important guarantee to achieve excellent performance synchronous pavement surface , which largely determines the design of synchronous pavement surface quality is good or bad . Thus the raw materials selection and testing work is very important .   

 1 , asphalt   

Synchronous chip seal technology , selection and use of asphalt in principle no special requirements . Ensuring proper asphalt spreaders temperature, spread quantities premise , the use of ordinary asphalt, heavy traffic asphalt , emulsified asphalt , modified asphalt can get very good results. It should be noted that the construction is to determine the amount of asphalt seal coat quality is good or bad is a very important factor . Too little of the seal coat asphalt road there may be a serious gravel threshing ; If excessive weeping phenomenon occurs . Therefore, the amount of asphalt to be based on traffic , road conditions , construction and other seasonal adjustments, such as a large amount of traffic on the road should be reduced by 5 % to 10% , with the ratio of the summer and autumn of construction should increase by about 5%.   

 2 , stone    

Stone is one of the important part of synchronous pavement surface , which is mainly exposed to the load of the vehicle, and to provide anti-slide driving role , which should be used in material quality stone . Synchronous pavement surface generally requires the use of counter-attack after crushing ( or hammer crusher ) the resulting rubble, flakiness content should be strictly limited to 15 % or less , and the geometry is better , free of impurities and powder , crushed value does not greater than 14% , and strictly dry after washing , while the stone pH no special requirements.